项目
Item |
指标
Indexes |
N-1 |
N-2a |
耐火度/Refractoriness (℃) |
1750 |
1730 |
2Kgf/cm2荷重软化开始温度 (℃)
Refractoriness under load |
≥1400 |
≥1350 |
重烧线变化 % 1400℃,2h
Permanent Linear Change |
-0.4 |
-0.3 |
显气孔率/Apparent Porosity % |
≤22 |
≤23 |
常温耐压强度/Cold crushing strength MPa
|
≥35 |
≥32 |
热震稳定性次数/Thermal shock resistance |
|
|
|
|
|